Inconel Pipe Grades at a Glance
Choosing an Inconel pipe comes down to grade and duty, not a single catch-all material. Nandini Steel stocks the four working grades and matches each one to the failure mode it's built to beat:
High-temperature oxidation and carburizing resistance mark out Inconel 600 and 601 (Ni-Cr-Fe). The aluminum addition in 601 pushes scaling resistance further, toward roughly 1180 °C, which suits furnace and heat-treatment work.
Inconel 625 (Ni-Cr-Mo) handles wet corrosion. Molybdenum and niobium together beat back chloride pitting, crevice attack, chloride stress-corrosion cracking, and sour service involving H2S.
Age-hardenable Inconel 718 (Ni-Cr-Fe) is precipitation-hardened to deliver very high mechanical strength, with tensile properties of 1275 MPa or above. That makes it the choice for oil-and-gas downhole work and rotating equipment.
All grades come in both seamless and welded forms (ERW/EFW), made to ASTM B167/B444. Stock is held ready for immediate dispatch, and every order ships with an EN 10204 3.1 mill test certificate.
As a stockist and supplier certified to ISO 9001:2015, with a focus on nickel alloys such as Incoloy 800 and the Hastelloy family, Nandini Steel supplies Inconel pipe cut from genuine mill plate and billet, with full heat traceability behind every order. Want the bigger picture on the material family? Our overview of nickel alloys covers it.
Inconel Pipe Grades & Designations
Each grade comes with a UNS number, a Werkstoff (W.Nr) number, an alloy family, and a clear rule for when to choose it. The metallurgy details for each grade sit on their own pages, linked right there in the table.
| Grade | UNS | W.Nr | Family | Choose when |
|---|---|---|---|---|
| Inconel 600 | N06600 | 2.4816 | Ni-Cr-Fe | General heat + corrosion; chloride-SCC resistance |
| Inconel 601 | N06601 | 2.4851 | Ni-Cr-Fe (+Al) | Oxidation / scaling resistance to ~1180 °C |
| Inconel 625 | N06625 | 2.4856 | Ni-Cr-Mo | Wet corrosion, chlorides, crevice, sour service |
| Inconel 718 | N07718 | 2.4668 | Ni-Cr-Fe (age-hardenable) | High mechanical strength, downhole / rotating duty |
Chemical Composition by Grade
Representative wrought compositions (weight %, balance nickel where shown). In 625, molybdenum and niobium drive the properties the grade is specified for; in 718, it's niobium, titanium and aluminum that do the work.
| Element | Inconel 600 | Inconel 601 | Inconel 625 | Inconel 718 |
|---|---|---|---|---|
| Ni | ≥72 | 58–63 | ≥58 | 50–55 |
| Cr | 14–17 | 21–25 | 20–23 | 17–21 |
| Fe | 6–10 | balance | ≤5 | balance |
| Mo | – | – | 8–10 | 2.8–3.3 |
| Nb+Ta | – | – | 3.15–4.15 | 4.75–5.5 |
| Al | – | 1.0–1.7 | – | 0.2–0.8 |
| Ti | – | – | – | 0.65–1.15 |
| C | ≤0.15 | ≤0.10 | ≤0.10 | ≤0.08 |
| Mn | ≤1.0 | ≤1.0 | ≤0.5 | ≤0.35 |
Mechanical Properties by Grade
Minimum room-temperature values in the supplied condition: 600, 601 and 625 solution-annealed. 718 in the precipitation-hardened, or aged, condition, which is what gives it its strength.
| Grade | Condition | Tensile (MPa) | 0.2% Yield (MPa) | Elongation (%) |
|---|---|---|---|---|
| Inconel 600 | Annealed | ≥550 | ≥240 | ≥30 |
| Inconel 601 | Annealed | ≥550 | ≥205 | ≥30 |
| Inconel 625 | Annealed | ≥827 | ≥414 | ≥30 |
| Inconel 718 | Aged | ≥1275 | ≥1034 | ≥12 |
Physical Properties
| Property | Inconel 600 | Inconel 601 | Inconel 625 | Inconel 718 |
|---|---|---|---|---|
| Density (g/cm³) | 8.47 | 8.11 | 8.44 | 8.19 |
| Melting range (°C) | 1354–1413 | 1301–1368 | 1290–1350 | 1260–1336 |
| Max continuous service (°C) | ~1095 | ~1180 | ~980 | ~700 |
Corrosion & Temperature Performance: Which Grade for Which Duty
Match the grade to the dominant failure mode. Don't just default to the best-known number.
- Dry high-temperature / oxidizing atmospheres: specify Inconel 601 for the highest scaling resistance (aluminum-stabilized oxide), with Inconel 600 for general heat and carburizing service, furnace retorts, radiant tubes and heat-treatment fixtures.
- Wet corrosion, chlorides and acids: Inconel 625 resists chloride pitting and crevice corrosion and chloride stress-corrosion cracking, and is qualified for sour service under NACE MR0175, it outperforms super-austenitic stainless in pitting resistance.
- High mechanical strength: Inconel 718 is the age-hardened choice where strength governs, such as downhole tubing and high-load components.
- Severe reducing acids: where hot concentrated acids exceed Inconel's envelope, step up to Hastelloy pipes; where the duty is milder, stainless steel pipes are the economical baseline.
"Inconel 825" Is Actually Incoloy 825
There's no Inconel 825. Buyers often write "Inconel 825" on inquiries when what they actually mean is Incoloy / Alloy 825 (UNS N08825), a Ni-Fe-Cr alloy. Getting the designation right on the purchase order and the mill certificate keeps receiving inspection from turning into a dispute. Route this requirement to Incoloy 825 (not Inconel 825). When the two are on the table for sour or mixed-acid duty, the Incoloy 825 vs Inconel 625 comparison is worth a look.
Equivalent Designations
| Grade | UNS | W.Nr (DIN) | Common DIN name |
|---|---|---|---|
| Inconel 600 | N06600 | 2.4816 | NiCr15Fe |
| Inconel 601 | N06601 | 2.4851 | NiCr23Fe |
| Inconel 625 | N06625 | 2.4856 | NiCr22Mo9Nb |
| Inconel 718 | N07718 | 2.4668 | NiCr19Fe19NbMo3 |
Available Forms, Sizes & Schedules
Inconel pipe comes both seamless and welded (ERW/EFW) across all four grades. Standard wall schedules span SCH 5S through XXS, available in nominal-bore and outside-diameter dimensioning, and supplied in random or cut lengths.
| Attribute | Range |
|---|---|
| Manufacture | Seamless and welded (ERW/EFW) |
| Grades | 600, 601, 625, 718 |
| Schedule | SCH 5S – XXS |
| Standards | ASTM B167 / B444 (ASME SB-equivalents) |
| Availability | Ex-stock, immediate dispatch |
For an exact OD, nominal bore, and schedule against your line-list, send the requirement over by RFQ. Use the weight calculator to estimate pipe mass by grade and dimension.
Standards & Specifications Complied
Inconel pipe comes supplied to the governing ASTM/ASME specifications for each grade.
- Inconel 600 / 601: ASTM B167 (seamless Ni-Cr-Fe pipe) and ASME SB-167.
- Inconel 625: ASTM B444 / ASME SB-444 (seamless) and ASTM B705 (welded).
- Inconel 718: ASTM B637 / AMS bar-and-tube specifications for age-hardenable grades.
- Sour service: heats qualified to NACE MR0175 / ISO 15156 for 625 and 718 where specified on the order.
Testing, Inspection & Certification
Every Inconel pipe order comes with an EN 10204 3.1 (or 3.2 on request) mill test certificate that ties the pipe to its heat and cast number. For what that document actually records, see EN 10204 3.1 mill test certificate. Verification as standard covers positive material identification (PMI), hydrostatic testing, ultrasonic (UT) inspection, and intergranular corrosion testing per ASTM A262/G28. The full scope is laid out in our note on testing, MTC, NDT and PMI. Where corrosion performance hinges on it, the solution-annealing condition gets confirmed right on the certificate. Background on that is in solution annealing.
Material's cut from genuine mill product, Aperam, Outokumpu, Jindal, POSCO, Nippon Steel, JFE where applicable. Third-party inspection can be arranged too, through TÜV SÜD, Bureau Veritas, DNV, SGS or ABS.
Applications of Inconel Pipe
Oil and gas, sour service: Inconel 625 line pipe and 718 downhole tubing for wells and flowlines carrying H2S and chlorides.
Chemical and acid processing: 625 piping for aggressive wet-corrosion duty. Think reactors, scrubbers, acid transfer lines, anywhere stainless steel pits.
High-temperature and furnace service: 601 and 600 tubes handle heat-treatment furnaces, petrochemical heaters, and carburizing atmospheres.
FAQ
Which Inconel pipe grade should I choose?
Are Inconel pipes available seamless and welded?
Is "Inconel 825 pipe" the same as Inconel 625?
What certification comes with Inconel pipe?
How is Inconel pipe priced?
Request a Quote
Nandini Steel has carried ISO 9001:2015 certification since 2003, stocking, supplying and exporting Inconel and nickel-alloy pipe for more than 20 years now. Every grade sits ex-stock, ready to ship right away, and each order comes with an EN 10204 3.1/3.2 mill test certificate.
Send your Inconel pipe requirement over, grade, seamless or welded, OD/NB, schedule, length and quantity, and we'll get back to you with live pricing and availability:
- Phone: +91 22 43404600 · +91 9920209184
- WhatsApp: +91 99202 09184
- Email: reachus@nandinisteel.com
- GSTIN: 27ADJPA7240C1Z0
- Address: 25, Dreamland Building, 601, 6th Floor, Mama Parmanand Marg, Charni Road, Opera House, Girgaon, Mumbai, Maharashtra 400004, India